This technical note describes the workshop method used by CNCGLASS to cut PDLC film and to make the electrode. The sequence covers sheet cutting on a double-position table, preparation of the film edge, silver-paste work on the screen, formation of the electrodes with copper mesh, conductive glue and copper foil, a lead-wire connection method, and a power-on test. A list of the tools and consumables is included, together with workshop details such as a 5 mm edge width, removal of the protective layer for about 6 cm, a 10-minute stir of the silver paste, and, for large-size film, a curing machine set to 113 degrees with a 10-minute bake. Enquiries can be sent to cnc@cncglass.com.